ASTM A213 Boiler Tube

For manufacture wall panel economizer, Re-heater, Super heater and stem pipe line of boilers.
Standard Steel Grade: ASME/ASTM SA/A213/T5/T11/T12/T22/T91

Product Details

  • Size Range

O.D 1/4″-24″; W.T SCH10-SCH160;

  • Chemical Composition Limits, %4 , for Low Alloy Steel
Chemical Composition Limits, %4 , for Low Alloy Steel
Grade UNS
Designatlion
Composition, %
Carbon Manganese Phosphorus Sulfur Silicon Nickel Chromium Molybdenum Vana-
dium
Boron Niobium Nitrogen Aluminum Tungsten
T2 K11547 0.10-0.20 0.30-0.61 0.025 0.025B 0.10-0.30 … 0.50-0.81 0.44-0.65 … … … … … …
T5 K41545 0.15 0.30-0.60 0.025 0.025 0.50 … 4.00-6.00 0.45-0.65 … … … … … …
T9 K90941 0.15 0.30-0.60 0.025 0.025 0.25-1.00 … 8.00-10.00 0.90-1.10 … … … … … …
T11 K11597 0.05-0.15 0.30-0.60 0.025 0.025 0.50-1.00 … 1.00-1.50 0.44-0.65 … … … … … …
T12 K11562 0.05-0.15 0.30-0.61 0.025 0.025B 0.50 … 0.80-1.25 0.44-0.65 … … … … … …
T17 K12047 0.15-0.25 0.30-0.61 0.025 0.025 0.15-0.35 … 0.80-1.25 … 0.15 … … … … …
T21 K31545 0.05-0.15 0.30-0.60 0.025 0.025 0.50-1.00 … 2.65-3.35 0.80-1.06 … … … … … …
T22 K21590 0.05-0.15 0.30-0.60 0.025 0.025 0.50 … 1.90-2.60 0.87-1.13 … … … … … …
T23 K40712 0.04-0.10 0.10-0.60 0.030 0.010 0.50 0.40 1.90-2.60 0.05-0.30 0.20-0.30 0.0010-0.006 0.02-0.08 0.015 0.030 1.45-1.75
T24 K30736 0.05-0.10 0.30-0.70 0.020 0.010 0.15-0.45 … 2.20-2.60 0.90-1.10 0.20-0.30 0.0015-0.007 … 0.012 0.02 …
T36 K21001 0.10-0.17 0.80-1.20 0.030 0.025 0.25-0.50 1.00-1.30 0.30 0.25-0.50 0.02 … 0.015-0.045 0.02 0.05 …
T91 K900901 0.07-0.14 0.30-0.60 0.020 0.010 0.25-0.50 0.40 8.0-9.5 0.85-1.05 0.18-0.25 … 0.06-0.10 0.030-0.070 0.02 …
T92 K92460 0.07-0.13 0.30-0.60 0.020 0.010 0.50 0.40 8.5-9.5 0.30-0.60 0.15-0.25 0.001-0.006 0.04-0.09 0.030-0.070 0.02 1.5-2.00
T122 K91271 0.07-0.14 0.70 0.020 0.010 0.50 0.50 10.0-11.5 0.25-0.60 0.15-0.30 0.0005-0.005 0.04-0.10 0.040-0.100 0.02 1.50-2.50
T911 K91061 0.09-0.13 0.30-0.60 0.020 0.010 0.10-0.50 0.40 8.5-9.5 0.90-1.10 0.18-0.25 0.0003-0.006 0.06-0.10 0.040-0.090 0.02 0.90-1.10
  • Hardness Requirements:
  • Brinell, Vickers, or Rockwell hardness tests shall be

made on specimens from two tubes from each lot.

  • Flattening Test- One flattening test shall be made on specimens from each end of one finished tube, not the one used for the flaring test, from each lot.
  • Flaring Test- _One flaring test shall be made on speci-mens from each end of one finished tube, not the one used for the fattening test, from each lot.
  • Mechanical property requirements do not apply to tubing smaller than /8 in. [3.2 mm] in inside diameter or thinner than 0.015 in. [0.4 mm] in thickness.

ASTM A213 Boiler Tube