- 尺寸范围
O.D 1/4″-24″; W.T SCH10-SCH160;
- Chemical Composition Limits, %4 , for Low Alloy Steel
Chemical Composition Limits, %4 , for Low Alloy Steel | |||||||||||||||
等级 | UNS Designatlion | 构成,% | |||||||||||||
Carbon | 锰 | Phosphorus | Sulfur | 硅 | 镍 | 铬 | Molybdenum | Vana- dium | Boron | Niobium | Nitrogen | 铝质 | Tungsten | ||
T2 | K11547 | 0.10-0.20 | 0.30-0.61 | 0.025 | 0.025B | 0.10-0.30 | … | 0.50-0.81 | 0.44-0.65 | … | … | … | … | … | … |
T5 | K41545 | 0.15 | 0.30-0.60 | 0.025 | 0.025 | 0.50 | … | 4.00-6.00 | 0.45-0.65 | … | … | … | … | … | … |
T9 | K90941 | 0.15 | 0.30-0.60 | 0.025 | 0.025 | 0.25-1.00 | … | 8.00-10.00 | 0.90-1.10 | … | … | … | … | … | … |
T11 | K11597 | 0.05-0.15 | 0.30-0.60 | 0.025 | 0.025 | 0.50-1.00 | … | 1.00-1.50 | 0.44-0.65 | … | … | … | … | … | … |
T12 | K11562 | 0.05-0.15 | 0.30-0.61 | 0.025 | 0.025B | 0.50 | … | 0.80-1.25 | 0.44-0.65 | … | … | … | … | … | … |
T17 | K12047 | 0.15-0.25 | 0.30-0.61 | 0.025 | 0.025 | 0.15-0.35 | … | 0.80-1.25 | … | 0.15 | … | … | … | … | … |
T21 | K31545 | 0.05-0.15 | 0.30-0.60 | 0.025 | 0.025 | 0.50-1.00 | … | 2.65-3.35 | 0.80-1.06 | … | … | … | … | … | … |
T22 | K21590 | 0.05-0.15 | 0.30-0.60 | 0.025 | 0.025 | 0.50 | … | 1.90-2.60 | 0.87-1.13 | … | … | … | … | … | … |
T23 | K40712 | 0.04-0.10 | 0.10-0.60 | 0.030 | 0.010 | 0.50 | 0.40 | 1.90-2.60 | 0.05-0.30 | 0.20-0.30 | 0.0010-0.006 | 0.02-0.08 | 0.015 | 0.030 | 1.45-1.75 |
T24 | K30736 | 0.05-0.10 | 0.30-0.70 | 0.020 | 0.010 | 0.15-0.45 | … | 2.20-2.60 | 0.90-1.10 | 0.20-0.30 | 0.0015-0.007 | … | 0.012 | 0.02 | … |
T36 | K21001 | 0.10-0.17 | 0.80-1.20 | 0.030 | 0.025 | 0.25-0.50 | 1.00-1.30 | 0.30 | 0.25-0.50 | 0.02 | … | 0.015-0.045 | 0.02 | 0.05 | … |
T91 | K900901 | 0.07-0.14 | 0.30-0.60 | 0.020 | 0.010 | 0.25-0.50 | 0.40 | 8.0-9.5 | 0.85-1.05 | 0.18-0.25 | … | 0.06-0.10 | 0.030-0.070 | 0.02 | … |
T92 | K92460 | 0.07-0.13 | 0.30-0.60 | 0.020 | 0.010 | 0.50 | 0.40 | 8.5-9.5 | 0.30-0.60 | 0.15-0.25 | 0.001-0.006 | 0.04-0.09 | 0.030-0.070 | 0.02 | 1.5-2.00 |
T122 | K91271 | 0.07-0.14 | 0.70 | 0.020 | 0.010 | 0.50 | 0.50 | 10.0-11.5 | 0.25-0.60 | 0.15-0.30 | 0.0005-0.005 | 0.04-0.10 | 0.040-0.100 | 0.02 | 1.50-2.50 |
T911 | K91061 | 0.09-0.13 | 0.30-0.60 | 0.020 | 0.010 | 0.10-0.50 | 0.40 | 8.5-9.5 | 0.90-1.10 | 0.18-0.25 | 0.0003-0.006 | 0.06-0.10 | 0.040-0.090 | 0.02 | 0.90-1.10 |
- Hardness Requirements:
- Brinell, Vickers, or Rockwell hardness tests shall be
made on specimens from two tubes from each lot.
- Flattening Test- One flattening test shall be made on specimens from each end of one finished tube, not the one used for the flaring test, from each lot.
- Flaring Test- _One flaring test shall be made on speci-mens from each end of one finished tube, not the one used for the fattening test, from each lot.
- Mechanical property requirements do not apply to tubing smaller than /8 in. [3.2 mm] in inside diameter or thinner than 0.015 in. [0.4 mm] in thickness.
联系我们
项目方案
- 锅炉 & 容器
- EPC 成套设备(管件和法兰)
- 离岸应用
- 石油天然气管道
- 石油化工
产品
- 翅片管
- 锅炉产品
- 管道预制
- 板式热交换器
- 法兰
- 钢管
联系我们
海外代表处:Sunwen Project Oman LLC
无锡尚文工业有限公司版权所有 © 2024
无锡尚文管业有限公司 & 无锡尚文管业有限公司